Furnace lining manufacturers tell you the operation steps of the oven
Today, Luoyang Quantong Kiln Industry Co., Ltd., a furnace lining manufacturer, tells you the operation steps of the furnace:
1. Reminder of gravity furnace lining materials. First, cover the crucible mold with asbestos cloth or furnace cover, leaving only one vent hole, so that the entire furnace lining can be heated evenly, so as to facilitate the overall sintering.
2. It takes 2 hours to slowly heat the furnace to 600 degrees Celsius, keep it here for 1 hour, and then slowly heat the furnace to 1000 degrees Celsius, which takes 2 hours, and keep it here for 1 hour.
3. After the furnace temperature is naturally cooled to room temperature, step on the furnace mold with your feet, lightly hit the furnace with a hammer to make it vibrate and have a gap with the furnace wall, then slowly take out the furnace mold.
4. Check whether the furnace wall has fallen off. If it falls off slightly, it can be repaired by adding glass water and water to the furnace lining material. If it falls off seriously, it means that the furnace wall is not tight enough, and the furnace needs to be rebuilt.
5, Put the iron blocks into the furnace densely by hand.
6. The furnace must be fully sintered, and the liquid level should be about 100mm away from the furnace mouth, so as to facilitate the overall sintering.
7. In the first furnace, the acid lining material is slowly heated and melted, and kept at 1580 degrees Celsius (±20 degrees Celsius) for half an hour.
When the molten iron temperature is greater than 1500 degrees Celsius, the temperature is generally monitored every 10 minutes.
Start charging when the initial charge is melted to about 30%.
Each feeding should be carried out before the last feeding is not completely melted, be careful not to cause the phenomenon of shedding, and continue feeding until the furnace is full.
8. The occurrence of hanging material during the smelting process should be dealt with in time:
Luoyang Quantong Kiln Industry Co., Ltd. is a comprehensive high-tech company integrating R&D, production, sales and construction services. It is a high-tech enterprise in Henan Province and an IS09001 quality assurance system certification enterprise. We sincerely welcome your inquiries.
Previous: Analysis of Corrosion Phenomenon of Furnace Surface Lining
下一条: What are the special advantages of using coil insulating glue?
Related Industry Knowledge
- Features and Benefits of Coil Clay
- What are the advantages of a good furnace lining
- Misunderstandings in the use of ramming materials in intermediate frequency furnaces
- Phenomenon analysis of failure of argon blowing of ladle permeable bricks and how to improve the rate of argon blowing
- Where is the consumption reduction and energy saving of breathable bricks reflected?
- How to improve the service life of intermediate frequency furnace lining
- Reasons for damage to intermediate frequency furnace lining and how to solve them
- The performance and advantages of breathable brick
- Analysis of Structural Characteristics of Dispersive Breathable Bricks
- The intermediate frequency furnace charge knotting process needs to pay attention to details sharing
- Analysis of Corrosion Phenomenon of Furnace Surface Lining
- Why does the intermediate frequency furnace lining have cracks?
- Cause Analysis of Damaged Refractory Material of Submerged Arc Furnace Lining
- Will the ramming material attack chemically?
- Do you know how to choose the correct acid furnace lining
- How to repair the electric furnace lining
- What should be paid attention to when lining the furnace
- Introduction of ramming material for intermediate frequency furnace
- Influence of medium frequency electric furnace lining material
- How to build furnace and sintering process for intermediate frequency furnace lining materials